Now we discuss the pros and cons of sending a flashed manifold out for repair versus performing this task in-house. This article will begin to deal with the disassembly, troubleshooting, cleaning and reassembling of a typical, and flashed 16-cavity valve gate manifold.
Obviously there are many different makes of hot runner manifolds currently being used in the making of plastic parts today. Relevant (and most critical) design differences that will affect a manifold’s potential to leak concerns how the nozzles, sprue and any cross-overs (or bridges) are connected to the manifolds. These components are either bolted to, threaded into or rely on a compression stack, and sometimes a combination of all three. Each type has its trade-offs concerning required maintenance of the system and the overall ease of installing replacement parts, such as thermocouples, nozzles, nozzle tips and heaters.
Regardless of flowery forecasts made by manifold sales folks, the ease at which a manifold system can be maintained will not be apparent until the system has some hours on it (a million cycles would be nice), giving internal components, pockets and tooling clearances time to collect vent residue (greasy film or powders) and weepage (gooey, degraded plastic).
Also impacting manifold condition are molds stressed through weekend shut-downs and hurried Monday morning start-ups along with touchy gate/valve pin tip configurations that promote out-of-spec gate vestiges—forcing processors to fiddle with the parameters.
Some systems require a complete teardown just to replace a nozzle heater or thermocouple. On others, if specific components are disturbed or removed they too must be completely disassembled and cleaned before reassembly to ensure proper component stack dimensions.
The level of disassembly/reassembly (labor hours and skill level) required over time to replace basic components along with the usage (cost) of the components will determine the true ease of maintenance with the system.
But obviously, any manifold that encapsulates easily (easily meaning that if a strict start-up procedure is not followed to the letter, the system has the capability to blow at multiple locations) will not be a popular choice among those of us who have to fix or run them.
For the sake of fairness and consistency, we will examine areas of concern regardless of the manifold make and model.
In manifold maintenance, the same five basic principles that apply to a mold also apply to an encapsulated manifold. The only difference is that troubleshooting the source of the leak could be ongoing throughout the repair process as plastic is removed and more tooling is exposed—allowing better visual inspection of seal areas and components, right up through assembly of the cleaned components.
Here is an overview of the five basic steps that will occur on an encapsulated system:
1. Disassemble
Remove the valve pins and clamp plate, and disassemble mold to gain visual access to the back of manifold.
Pay attention to tooling clues that can point to the leak source (bent, broken or galled valve pins and the amount and type of residue around the pin).
Remove enough plastic as to facilitate separating the manifold and electrical box from the plate, so that you can clean these components separately.
2. Clean
Clean clamp plate, manifold plate channels, counter-bores and valve pins (ultrasonic).
Clean nozzles, heater and thermocouple wires and manifold (by hand).
3. Troubleshoot
Inspect seal areas of components for obvious cracks and plates for hobbing and bolts for looseness.
4. Assemble
Reassemble to stage one.
Electrical check.
Final reassembly to stage two.
5. Final Check
Electrical check ramping heaters up to processing temp with water flowing through appropriate channels.
Let’s begin with the mold in the press. The first noticeable sign of a flashed manifold is usually when smoke is seen rising from the top of the stationary side, or plastic oozing from places it shouldn’t … then the panic and finger pointing ensues.
But there are other, more subtle clues that might point to a manifold leak, such as molds that produce periodic incomplete shots, shorted out heaters and thermocouples in a particular quadrant.
Paying attention to these signs can alert a processor to a possible manifold malfunction and allow them to shut a mold down before the manifold is totally encapsulated.
Our new Hot Runner Manifold Cleaning System is the fastest, most cost saving and environmentally friendly method of removing practically all organic contaminants such as plastic, rubber or paint from steel parts. we have taken mold maintenance to a new level with the addition of our Mold Manifold and Hot Runner Cleaning System. With this operation, parts are loaded into a tank where fluidized hot sand at a temperature of 800 to 850 degrees Fahrenheit, scrubs, vaporizes, and burns off all left over organic material without damaging or warping the work pieces. The basket of cleaned parts is then hoisted out of the tank and set to cool. Now we are truly able to inspect and evaluate your jobs specific situation then dissect and address the issues necessary.
Repair technicians must be properly trained in hot runner characteristics so that companies are not experiencing unnecessarily long and expensive downtime hours while waiting to get a mold return from an outside vendor. repairing and maintaining a typical hot runner system takes maintenance skills to the next level. successful hot runner repair requires a higher level of understanding, concerning how they function and their critical areas that need to be monitored. safe, precise, and reliable repairs can only be accomplished in a methodical approach that utilizes accurate documentation and a thorough knowledge base that guides technicians through specific procedures during maintenance and repair work. tooling in a typical hot runner system must be handled with great care while cleaning inspecting and reassembling. specific practices and techniques must be used to prevent potential flooding or encapsulation disasters that can plague all hot runner systems. also discussed are various processing techniques and resins that can have a huge effect on the performance, condition, and maintenance practices of a hot runner system. the cleaning procedure of manifold cleaning, refurbishment, electrical on hot runner systems is crucial.
When using an injection mould tool with a Hot Runner System it is sometimes necessary to clean the system due to misuse.Typical examples of situations that result in the manifold requiring cleaning are as follows:
Manifolds Left With Power On For Extended PeriodsMany older moulding machines will not power down the heaters when the machine is shut-off, so manifolds are left to overheat. This will result in two things:
1. The overheated plastic is significantly reduced in viscosity causing the resin (weepage) to migrate into tooling clearances.
2. The tooling overheats, causing the manifold to over-expand and hob sealing surfaces, reducing the ability to seal when the manifold temperature is brought back down into range.If the plastic resin that is being processed is sensitive to heat, an engineering grade or a filled material then serious overheating can result in the material crystallising inside the melt channels of the Hot Runner System and is unable to be re-melted.
Process Habits
Failing to reduce shot size when blocking cavities, not using back pressure when filling empty manifolds, running temps to high, reversing valve pin sequence and forgetting to turn on the cooling are just a few of several processing conditions that contribute to leaking systems.
Lack of Preventative Maintenance
Worn valve pins and bushings seem to be a major contributor, particularly where manifolds are long overdue for thorough maintenance. Also lethal are hobbed manifolds, spacers and other tooling where combined dimensions are under the recommended cold stack height. This also includes stressed/stretched bolts.
Cleaning Processes
There are many processes available to assist you with thorough cleaning of a manifold. Depending on the complexity of your manifold it is often impossible to properly clean the channels inside a manifold simply by removing plugs and removing the plastic.
There are two choices for cleaning up the system: the first choice is to send it to a qualified service center where the system will be placed in an oven at high temperatures to burn off the excess plastic. the advantage of this method is a fast turnaround with new thermocouples and heaters. the disadvantage is cost. new thermocouples and heaters are expensive. time is also a factor, the second choice is to clean it in-house. this option can save thousands of dollars, including a 50% to 75% savings just in thermocouples and heaters. a determination also can be made from where the leak came from. knowledge can be gained on how to prevent future leaks and the overall operation of the system. house repairs properly executed will always save time and money. cleaning and repairing an encapsulated system also requires a higher skill level to troubleshoot, clean, and reassemble without further damage. failing to do this correctly can cause the system to flood again. due to an unrelated issue that caused the first flooding. many hot runner manifold problems can be traced back to a lack of knowledge concerning hot runner assembly mistakes, poor work habits, improper tools use during the clean and repair of the manifold, and critical components.
1) Open gate
1 cleanup barrel by plastic material with demand color.
2 heat each heating zone with the temperature by 15-20 ℃ over normal production temperature.
3 shot 10-15 times according to normal procedure.
4 move back the the injection unit (barrel),turn off the hot runner system.
5 cool down the hot runner system, which method leads to the shrinkage of hot plastic material in the runner channel due to the reduced temperature , and then separated from the channel so the old and new materials could be mixed.
6 turn on the hot runner system again and wait until the temperature rise to production demand.
7 move back barrel.
8 increase the injection speed and repeat injection molding procedure until the color of the product can be accepted.
9 gradually restore the process of setting , restore injection speed and temperature to original production process demand.
2) Valve gate
1 the hot-runner system has processed plastic material with a certain color.
2 cleanup barrel by plastic material with demand color .
3 heat each heating zone with the temperature by 15-20 ℃ over normal production Temperature .
4 shot 10-15 times according to normal procedure to clean the barrel (Note:unless hot runner reached the plastic processing temperature ,valve needle need to keep its position otherwise the valve needle and gates could be damaged when clean the barrel.)
5 move back the the injection unit (barrel),turn off the hot runner system.
6 cool down the hot runner system, which method leads to the shrinkage of hot plastic material in the runner channel due to reduced temperature , and then separated from the channel so the old and new materials could be mixed.
7 turn on the hot runner system again and wait until the temperature rise to production demand.
8 move back barrel.
9 increase the injection speed and repeat injection molding procedure until the color of the product can be accepted
10 gradually restore the process of setting , restore injection speed and temperature to original production process demand.
3) Dismantle and Clean the residual mixed color material inside hot runner . Check the injection molding machine nozzle and hot runner gate for the mixed color residual material and repeat the injection to clean that material.
There are many processes available to assist you with thorough cleaning of a set of hot runner system. Depending on the complexity of your manifold and hot runners. it is often impossible to properly clean the channels inside a manifold simply by removing plugs and removing the plastic.
Elaborate tools are used in injection molding which require regular cleaning. Screw tips, injection nozzles, static mixers and especially hot-runner systems require extremely reliable polymer removal. I am sure to have such thermal cleaning technologies guarantee such removal. Even sprayed over hot-runner distributors with complicated geometries and glass fiber contents can be cleaned gently and without residues of polymer and carbon remnants as well as inorganic contaminations.
Today’s use of hot-runner technology allows the injection molding of very complex and large components. However, the sometimes very long internal flow channels make manual cleaning impossible; the use of rinsing chemicals usually produces only inadequate results. Even for sprayed over hot-runners / hot-runner nozzles thermal cleaning is the only solution.
we have taken mold maintenance to a new level with the addition of our Mold Manifold and Hot Runner Cleaning System. With this operation, parts are loaded into a tank where fluidized hot sand at a temperature of 800 to 850 degrees Fahrenheit, scrubs, vaporizes, and burns off all left over organic material without damaging or warping the work pieces. The basket of cleaned parts is then hoisted out of the tank and set to cool. Now we are truly able to inspect and evaluate your jobs specific situation then dissect and address the issues necessary. any question, please contact
I once attended a seminar where the guest speaker was a hot-runner specialist who thanked us in the audience for our continued support of his children’s college fund through our steady tendency to encapsulate manifold wiring and other delicate components with flash. When asked reasons for these flashing follies, he cited these causes in order of frequency:
1) Manifolds left on over weekends. Many older presses will not power down the heaters when the press is shut off, so manifolds are left to cook. This accomplishes two things: The overheated plastic de grades and drops significantly in viscosity, causing resin weepage into tooling clearances. Second, the tooling overheats, causing it to expand and hob the sealing surfaces, reducing the manifold’s ability to seal itself when the temperature is brought back down into proper range.
2) Cold starts. His college fund loves impatient molders who don’t allow manifolds adequate “soak” time of 20 to 40 min to allow the steel to fully expand and create the necessary sealing pressure between components.
3) Bad processing habits. Failing to reduce shot size after blocking cavities, not using backpressure when filling empty manifolds, running temperatures too high, reversing valve-pin sequence, and forgetting to turn on the cooling water are just a few deadly sins that contribute to leaking systems.
4) Lack of preventive maintenance. Worn valve pins and bushings are common in manifolds that are overdue for a thorough going over.
5) Also lethal are hobbed manifolds, spacers, and other tooling whose combined di men sions are under the recommended cold stack height. Other culprits are stressed or stretched bolts and fatigued compression-seal washers.
6) Short cuts. Too often, in-house manifold cleanings are attempted by personnel who, for the sake of speed and dollars (or due to inexperience), try short cuts like partial disassembly and cleaning, or they fail to assemble the manifold correctly. It takes only a small mistake, such as a bolt that is not properly torqued or a probe skirt not fully seated, to create a clearance that allows melt to leak.
7) Cracked tooling. Manifolds, probes, sprues, and crossover bars/ bridges can develop small fractures that turn into major cracks under injection pressure.
8) Bad design. When shopping for a hot-runner system, it would be great to inspect one that has run a few million cycles—but you don’t see these at trade shows. Too bad.