Now we discuss the pros and cons of sending a flashed manifold out for repair versus performing this task in-house. This article will begin to deal with the disassembly, troubleshooting, cleaning and reassembling of a typical, and flashed 16-cavity valve gate manifold.
Obviously there are many different makes of hot runner manifolds currently being used in the making of plastic parts today. Relevant (and most critical) design differences that will affect a manifold’s potential to leak concerns how the nozzles, sprue and any cross-overs (or bridges) are connected to the manifolds. These components are either bolted to, threaded into or rely on a compression stack, and sometimes a combination of all three. Each type has its trade-offs concerning required maintenance of the system and the overall ease of installing replacement parts, such as thermocouples, nozzles, nozzle tips and heaters.
Regardless of flowery forecasts made by manifold sales folks, the ease at which a manifold system can be maintained will not be apparent until the system has some hours on it (a million cycles would be nice), giving internal components, pockets and tooling clearances time to collect vent residue (greasy film or powders) and weepage (gooey, degraded plastic).
Also impacting manifold condition are molds stressed through weekend shut-downs and hurried Monday morning start-ups along with touchy gate/valve pin tip configurations that promote out-of-spec gate vestiges—forcing processors to fiddle with the parameters.
Some systems require a complete teardown just to replace a nozzle heater or thermocouple. On others, if specific components are disturbed or removed they too must be completely disassembled and cleaned before reassembly to ensure proper component stack dimensions.
The level of disassembly/reassembly (labor hours and skill level) required over time to replace basic components along with the usage (cost) of the components will determine the true ease of maintenance with the system.
But obviously, any manifold that encapsulates easily (easily meaning that if a strict start-up procedure is not followed to the letter, the system has the capability to blow at multiple locations) will not be a popular choice among those of us who have to fix or run them.
For the sake of fairness and consistency, we will examine areas of concern regardless of the manifold make and model.
In manifold maintenance, the same five basic principles that apply to a mold also apply to an encapsulated manifold. The only difference is that troubleshooting the source of the leak could be ongoing throughout the repair process as plastic is removed and more tooling is exposed—allowing better visual inspection of seal areas and components, right up through assembly of the cleaned components.
Here is an overview of the five basic steps that will occur on an encapsulated system:
1. Disassemble
Remove the valve pins and clamp plate, and disassemble mold to gain visual access to the back of manifold.
Pay attention to tooling clues that can point to the leak source (bent, broken or galled valve pins and the amount and type of residue around the pin).
Remove enough plastic as to facilitate separating the manifold and electrical box from the plate, so that you can clean these components separately.
2. Clean
Clean clamp plate, manifold plate channels, counter-bores and valve pins (ultrasonic).
Clean nozzles, heater and thermocouple wires and manifold (by hand).
3. Troubleshoot
Inspect seal areas of components for obvious cracks and plates for hobbing and bolts for looseness.
4. Assemble
Reassemble to stage one.
Electrical check.
Final reassembly to stage two.
5. Final Check
Electrical check ramping heaters up to processing temp with water flowing through appropriate channels.
Let’s begin with the mold in the press. The first noticeable sign of a flashed manifold is usually when smoke is seen rising from the top of the stationary side, or plastic oozing from places it shouldn’t … then the panic and finger pointing ensues.
But there are other, more subtle clues that might point to a manifold leak, such as molds that produce periodic incomplete shots, shorted out heaters and thermocouples in a particular quadrant.
Paying attention to these signs can alert a processor to a possible manifold malfunction and allow them to shut a mold down before the manifold is totally encapsulated.
Follow these step-by-step instructions when using an purging compound mechanical grade to clean hot runner systems with mold plates open:
1) After the screw and barrel have been cleaned thoroughly using the purging compound, set the nozzle into the mold.
2) Open the mold plates.
3) Set up a safety-approved surface for collecting the purgings.
4) Verify that the mold safety door is closed.
5) Add enough purging compound into the hopper to fill the barrel approximately ½ full.
6) Extrude the purging compound through the hot runner system starting at a medium velocity. Increase screw speed to the maximum safe level for maximum cleaning. Once it is flowing adequately through all of the gates, perform injection shots (air shots) with mold plates open.
7) Visually inspect purgings for color and/or carbon contamination.
If contamination remains, repeat steps 5 through 7 until the purging compound is visually free of color and/or carbon contamination and has returned to a clean appearance.
8) Purge out any remaining using the maximum safe screw speed.
9) Adjust the temperatures in the barrel and hot runners to the processing conditions for the next resin to be processed.
10) Flush the system with the next resin to be processed using the maximum safe screw speed until the next resin is visually free of the purging compound.
Resume production using normal production settings.
I have spent hundreds of hours chipping and cleaning manifolds of 16- to 48-cavity molds with various types of manifold systems. Some may flash easier than others, but none is immune to flashing caused by a hurried start-up by an impatient molder or caused by bolts left loose by a preoccupied repair tech. No particular brand of manifold cleans up more quickly or easily than any other. But every flashed system seems to attract a number of white shirts clamoring for a super-quick turnaround, with no apparent clue as to what the job entails.
Proven Methods And Best Practices:
Unfilled grades of ASACLEAN can pass through the same clearances as the resins being processed.
Filled ASACLEAN grades (EX, PX2 and NF are not usually recommended for hot runner cleaning. Consult Sun Plastech Inc. for guidance on using filled grades for purging hot runners.
External heating systems: Raise the manifold temperature to 20°C – 30°C (35°F – 55°F) for improved flow. If running heat-sensitive resins, do not exceed the maximum safe operating temperature of the material.
Internal heating systems: Consult with a Purging Process Expert for technical assistance before using ASACLEAN.
If available, apply mold release agent to reduce the potential for material sticking to the mold surface.
Preparation: The entire hot runner system temperature must be within the usage range of the ASACLEAN purging compound grade to be used.
Cleaning of hot runner systems using unfilled purging compound grades of ASACLEAN may now be performed. ASACLEAN purging compound that is run through hot runner channels combines with residual materials and removes them safely while leaving a minimal amount of ASACLEAN residue.
the optimal thermal cleaning method for any hot-runner size or geometry:
INNOVACLEAN – Fluidized bed pyrolysis for all polymers
MAXICLEAN – Pyrolysis systems for extra large components
VACUCLEAN – Gentle but efficient vacuum pyrolysis
The advantages of these systems are their excellent cleaning quality within very short cleaning periods, their suitability even for glass fiber-reinforced materials and their cleaning technology that is easy on materials and the environment.
Today’s use of hot-runner technology allows the injection molding of very complex and large components. However, the sometimes very long internal flow channels make manual cleaning impossible; the use of rinsing chemicals usually produces only inadequate results. Even for sprayed over hot-runners / hot-runner nozzles thermal cleaning is the only solution.
I have spent hundreds of hours chipping and cleaning manifolds of 16- to 48-cavity molds with various types of manifold systems. Some may flash easier than others, but none is immune to flashing caused by a hurried start-up by an impatient molder or caused by bolts left loose by a preoccupied repair tech. No particular brand of manifold cleans up more quickly or easily than any other. But every flashed system seems to attract a number of white shirts clamoring for a super-quick turnaround, with no apparent clue as to what the job entails.
After the dirty work is done, it will test the skills of the most seasoned craftsman to perform the precise measurements necessary to determine if combined tooling tolerances (stack-out) are enough to have contributed to the leak. Measuring mold components to within 0.0001 in. while referencing non-perfect surfaces is a time-consuming task requiring calibrated instruments, a surgeon’s touch, and excellent analytical skills. It is the part of the troubleshooting process that separates a journeyman from, well, everyone else.
Too often, in-house manifold cleanings are attempted by personnel who, for the sake of speed and dollars (or due to inexperience), try short cuts like partial disassembly and cleaning, or they fail to assemble the manifold correctly. It takes only a small mistake, such as a bolt that is not properly torqued or a probe skirt not fully seated, to create a clearance that allows melt to leak.
Cracked tooling. Manifolds, probes, sprues, and crossover bars/ bridges can develop small fractures that turn into major cracks under injection pressure.
Bad design. When shopping for a hot-runner system, it would be great to inspect one that has run a few million cycles—but you don’t see these at trade shows. Too bad.
Today’s use of hot-runner technology allows the injection molding of very complex and large components. However, the sometimes very long internal flow channels make manual cleaning impossible; the use of rinsing chemicals usually produces only inadequate results. Even for sprayed over hot-runners / hot-runner nozzles thermal cleaning is the only solution.
the optimal thermal cleaning method for any hot-runner size or geometry:
INNOVACLEAN – Fluidized bed pyrolysis for all polymers
MAXICLEAN – Pyrolysis systems for extra large components
VACUCLEAN – Gentle but efficient vacuum pyrolysis
The advantages of these systems are their excellent cleaning quality within very short cleaning periods, their suitability even for glass fiber-reinforced materials and their cleaning technology that is easy on materials and the environment.
Often referred to as runnerless molding or hot-manifold systems, hot runner molds describe a set of temperature control heating-devices installed in the mold. The purpose of a hot runner injection system is to maintain a molten flow of plastics or rubber from the injection molding machine nozzle to the gate in a plastic injection mold — keeping the runner above the melting point of the plastic.
Hot runner molding systems consist of two plates heated by a manifold system inside one-half of the mold that sends the melted material to nozzles, which feed the part cavities. The system consists of two parts: the hot manifold and the drops. The manifold moves the rubber on a single plane and parallel to the parting line to a location above the cavity. Positioned perpendicular to the manifold, the drops move the rubber from the manifold to the component.