Optimize mold design to avoid shrink mark

Properly increase section dimension of gate and runner; the position of gate is set at thick walls of the plastic parts and should be as symmetric as possible; improve mold exhausting condition; set cold-slug well with sufficient capacity to avoid cold material’s entering into the cavity and influencing filling and shrinkage compensation; […]

By |2020-07-12T14:56:01+08:00October 13th, 2015|Mirco Blog|0 Comments

Introduction to shrink mark and shrinkage porosity

Both the shrink mark and shrinkage porosity are defects of injection products due to the molding shrinkage at thick walls where no sufficient follow-up compensation is made. During the injection process, the surface layer of products often condenses first, followed by the center layer, which will cause sinking on the surface of parts with thick [...]

By |2025-04-22T16:00:28+08:00September 29th, 2015|Mirco Blog|2 Comments